| Gred | 1Cr13Al4 | TK1 | 0Cr25Al5 | 0Cr20Al6RE | 0Cr23Al5 | 0Cr19Al3 | 0Cr21Al6Nb | 0Cr27Al7Mo2 | |
| Komposisi nominal% | Cr | 12.0-15.0 | 22.0-26.0 | 23.0-26.0 | 19.0-22.0 | 22.5-24.5 | 18.0-21.0 | 21.0-23.0 | 26.5-27.8 |
| Al | 4.0-6.0 | 5.0-7.0 | 4.5-6.5 | 5.0-7.0 | 4.2-5.0 | 3.0-4.2 | 5.0-7.0 | 6.0-7.0 | |
| Re | sesuai | 0.04-1.0 | sesuai | sesuai | sesuai | sesuai | sesuai | sesuai | |
| Fe | Bal. | Bal. | Bal. | Bal. | Bal. | Bal. | Bal. | ||
| Nb0.5 | Mo1.8-2.2 | ||||||||
| Suhu operasi maksimum(°C) | 650 | 1400 | 1250 | 1250 | 1250 | 1100 | 1350 | 1400 | |
| Kerintangan 20 ℃(Ω/mm2/m) | 1.25 | 1.48 | 1.42 | 1.40 | 1.35 | 1.23 | 1.45 | 1.53 | |
| Ketumpatan(g/cm³) | 7.4 | 7.1 | 7.1 | 7.16 | 7.25 | 7.35 | 7.1 | 7.1 | |
| Kekonduksian Terma pada 20℃,W/(M·K) | 0.49 | 0.49 | 0.46 | 0.48 | 3.46 | 0.49 | 0.49 | 0.49 | |
| Pekali Pengembangan Linear(×10¯6/℃)20-1000℃) | 15.4 | 16 | 16 | 14 | 15 | 13.5 | 16 | 16 | |
| Anggaran Takat Lebur(℃) | 1450 | 1520 | 1500 | 1500 | 1500 | 1500 | 1510 | 1520 | |
| Kekuatan Tegangan (N/mm2 ) | 580-680 | 680-830 | 630-780 | 630-780 | 630-780 | 600-700 | 650-800 | 680-830 | |
| Pemanjangan(%) | ›16 | ›10 | ›15 | ›15 | ›15 | ›15 | ›15 | ›10 | |
| Kadar Pengecutan Variasi Bahagian(%) | 65-75 | 65-75 | 60-75 | 65-75 | 65-75 | 65-75 | 65-75 | 65-75 | |
| Frekuensi Bengkok Berulang (F/R) | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 | |
| Kekerasan(HB) | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | |
| Struktur Mikrograf | ferit | ferit | ferit | ferit | ferit | ferit | ferit | ferit | |
| Harta Magnetik | Magnet | Magnet | Magnet | Magnet | Magnet | Magnet | Magnet | Magnet | |
| Kehidupan Pantas(j/℃) | no | ≥80/1350 | ≥80/1300 | ≥80/1300 | ≥80/1300 | ≥80/1250 | ≥50/1350 | ≥50/1350 | |
150 0000 2421