| Gred | Ni% | Cu% | Al% | Ti% | Fe% | Mn% | S% | C% | Si% |
| Monel K500 | Min 63 | 27.0-33.0 | 2.30-3.15 | 0.35-0.85 | Maks 2.0 | Maks 1.5 | Maks 0.01 | Maks 0.25 | Maks 0.5 |
Spesifikasi
| Borang | Standard |
| Monel K-500 | UNS N05500 |
| Bar | ASTM B865 |
| wayar | AMS4676 |
| Lembaran/Pinggan | ASTM B865 |
| Menempa | ASTM B564 |
| Kawat Kimpalan | ERNiCu-7 |
Sifat Fizikal(20°C)
| Gred | Ketumpatan | Takat Lebur | Kerintangan Elektrik | Purata Pekali Pengembangan Terma | Kekonduksian Terma | Haba Tertentu |
| Monel K500 | 8.55g/cm3 | 1315°C-1350°C | 0.615 μΩ•m | 13.7(100°C) a/10-6°C-1 | 19.4(100°C) λ/(W/m•°C) | 418 J/kg•°C |
Sifat Mekanikal(20°C Min)
| Monel K-500 | Kekuatan Tegangan | Kekuatan Hasil RP0.2% | Pemanjangan A5% |
| Anil&Diumur | Min. 896 MPa | Min. 586MPa | 30-20 |
150 0000 2421